Mechanical Properties Metric English Comments
Adhesive Bond Strength >= 9.00 MPa
>= 1310 psi
ABS, Substrate Failure, Shear; ISO 4587
Permabond 170 Cyanoacrylate, gap filling
PERMABOND® 170 is a methyl cyanoacrylate adhesive. It is a single part, high viscosity liquid that will cure rapidly at room temperature when pressed into a thin film between parts. Permabond 170 w..
Adhesive Bond Strength >= 9.00 MPa
>= 1310 psi
ABS, Substrate Failure, Shear; ISO 4587
Permabond 2011 Cyanoacrylate, gel
PERMABOND® 2011 is a thixotropic, fast-setting cyanoacrylate particularly suitable for use on vertical and porous substrates. This material can be used on metals, plastics, elastomers, ceramics and..
Adhesive Bond Strength 9.00 MPa
1310 psi
Steel/steel after 3 mins, Shear
Permabond TA459 Toughened Acrylic Adhesive
Permabond TA459 is a structural acrylic adhesive designed primarily for bonding metals, ferrites, ceramics and some thermoplastics. This product was specifically designed to be non-corrosive to sens..
Adhesive Bond Strength 9.00 MPa
1310 psi
Steel/steel after 3 mins, Shear
Permabond TA4590 Toughened Acrylic Adhesive
Permabond TA4590 is a structural acrylic adhesive designed primarily for bonding metals, ferrites, ceramics and some thermoplastics. This product was specifically designed to be non-corrosive to sen..
Adhesive Bond Strength 9.00 - 10.0 MPa
1310 - 1450 psi
Glass/steel, Shear
Permabond UV620 UV-curable Adhesive
PERMABOND UV620 is a single part, fast curing, UV curable adhesive. Its excellent optical clarity and resistance to yellowing make it ideal for bonding glass and crystal for a high quality finish. I..
Adhesive Bond Strength >= 9.00 MPa
>= 1310 psi
Polycarbonate, Shear
Permabond UV645 UV-curable Adhesive
PERMABOND UV645 is a single part, fast curing, high viscosity UV curable adhesive designed specifically for bonding plastics. This material has excellent adhesion to a variety of plastics including ..
Adhesive Bond Strength >= 9.00 MPa
>= 1310 psi
Polycarbonate, Shear
Permabond UV649 UV-curable Adhesive
PERMABOND UV649 is a single part, fast setting, and UV curable adhesive designed specifically for bonding plastics. This material has excellent adhesion to a variety of plastics including polycarbon..
Adhesive Bond Strength 9.00 - 11.0 MPa
1310 - 1600 psi
FRP Glass/Epoxy, Shear; ASTM D1002
Permabond ES569 Epoxy Resin
PERMABOND® ES569 is a single-part heat cured epoxy adhesive with excellent adhesion to metal surfaces as well as composite materials. The high bond strength of this adhesive allows it to replace me..
Adhesive Bond Strength >= 9.00 MPa
>= 1310 psi
Polycarbonate, Shear
Permabond UV630 UV-curable Adhesive
PERMABOND UV630 is a single part, fast setting, and UV curable adhesive designed specifically for bonding plastics. This material has excellent adhesion to a variety of plastics including polycarbon..
Adhesive Bond Strength >= 9.00 MPa
>= 1310 psi
Phenolic, Substrate Failure, Shear; ISO 4587
Permabond 910FS Cyanoacrylate, Methyl grade
PERMABOND® 910FS is the original 100%-methyl cyanoacrylate adhesive. It is a single part, low viscosity liquid that will cure rapidly at room temperature when pressed into a thin film between parts..
Adhesive Bond Strength >= 9.00 MPa
>= 1310 psi
ABS, Substrate Failure, Shear; ISO 4587
Permabond 910FS Cyanoacrylate, Methyl grade
PERMABOND® 910FS is the original 100%-methyl cyanoacrylate adhesive. It is a single part, low viscosity liquid that will cure rapidly at room temperature when pressed into a thin film between parts..
Copyright © lookpolymers.com All Rights Reserved