Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 0.860 MPa | 125 psi | Typical lap shear |
Momentive Performance Materials RTV116 Red Adhesive Sealant, High Temperature Pourable One-part alkoxy cure. Typical uses: High-heat applications; encapsulate and seal heating elements.Data provided by the manufacturer, GE Silicones.GE Silicones became a part of Momentive Performance.. |
|||
Adhesive Bond Strength | 0.860 MPa | 125 psi | Typical lap shear |
Momentive Performance Materials RTV122 White Adhesive Sealant, General Purpose Paste One-part modified alkoxy cure. Modified alkoxy materials cure at room temperature and will outgas a small amount of ammonia and some alcohol during cure. Typical uses: General purpose for bonding .. |
|||
Adhesive Bond Strength | 0.860 MPa | 125 psi | Typical lap shear |
Momentive Performance Materials RTV123 Black Adhesive Sealant, General Purpose Paste One-part modified alkoxy cure. Modified alkoxy materials cure at room temperature and will outgas a small amount of ammonia and some alcohol during cure. Typical uses: General purpose for bonding .. |
|||
Adhesive Bond Strength | 0.860 MPa | 125 psi | Typical lap shear |
Momentive Performance Materials RTV128 Translucent Adhesive Sealant, General Purpose Paste One-part modified alkoxy cure. Modified alkoxy materials cure at room temperature and will outgas a small amount of ammonia and some alcohol during cure. Typical uses: General purpose for bonding .. |
|||
Adhesive Bond Strength | 0.860 MPa | 125 psi | Typical lap shear |
Momentive Performance Materials RTV5812 White Adhesive Sealant, Fast Cure Paste One-part modified alkoxy cure. Modified alkoxy materials cure at room temperature and will outgas a small amount of ammonia and some alcohol during cure. Typical uses: Fast-curing primerless adhes.. |
|||
Adhesive Bond Strength | 0.860 MPa | 125 psi | Typical lap shear |
Momentive Performance Materials RTV5813 Black Adhesive Sealant, Fast Cure Paste One-part modified alkoxy cure. Modified alkoxy materials cure at room temperature and will outgas a small amount of ammonia and some alcohol during cure. Typical uses: Fast-curing primerless adhes.. |
|||
Adhesive Bond Strength | 0.860 MPa | 125 psi | Typical lap shear |
Momentive Performance Materials RTV5818 Translucent Adhesive Sealant, Fast Cure Paste One-part modified alkoxy cure. Modified alkoxy materials cure at room temperature and will outgas a small amount of ammonia and some alcohol during cure. Typical uses: Fast-curing primerless adhes.. |