Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Adhesive Bond Strength = 55.2 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Adhesive Bond Strength 41.4 - 55.2 MPa

@Thickness 0.508 mm
6000 - 8000 psi

@Thickness 0.0200 in
1018 steel; ASTM C633-01
The NanoSteel® Company SHS 9172 TWAS Steel Alloy, Cored Wire
Coating Description: SHS 9172 TWAS is an iron based steel alloy with a nanoscale microstructure that features exceptional wear, corrosion and high temperature oxidation resistance in severe abrasion..