Mechanical Properties Metric English Comments
Adhesive Bond Strength 24.0 - 30.0 MPa
3480 - 4350 psi
Steel, Shear; ISO 4587
Permabond 731 Cyanoacrylate, toughened
PERMABOND® 731 is a toughened cyanoacrylate with very good impact and peel strength when compared to a conventional cyanoacrylate. It bonds rapidly at room temperature and its viscosity is stable o..
Adhesive Bond Strength 24.0 - 30.0 MPa
3480 - 4350 psi
Steel, Shear; ISO 4587
Permabond 735 Cyanoacrylate, toughened
PERMABOND® 735 is a toughened cyanoacrylate with very good impact and peel strength when compared to a conventional cyanoacrylate. It bonds rapidly at room temperature and its viscosity is stable o..
Adhesive Bond Strength 20.0 - 30.0 MPa
2900 - 4350 psi
Mild steel, Shear; ISO 4587
Permabond ET5401 Epoxy Resin
PERMABOND® ET5401 is a two-part, 2:1 mixable, semi-flexible toughened no slump epoxy adhesive with good adhesion to a variety of substrates such as wood, metal, ceramics and some plastics and compo..