Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 14.0 - 27.0 MPa | 2030 - 3920 psi | Zinc, Shear; ASTM D1002 |
Permabond ES550 Epoxy Resin PERMABOND ES550 is a single-part epoxy paste which is slump-resistant (does not flow) during cure. The adhesive is toughened for maximum impact resistance, along with excellent peel and shear streng.. |
|||
Adhesive Bond Strength | 14.0 - 27.0 MPa | 2030 - 3920 psi | Aluminum, Shear; ISO 4587 |
Permabond ES562 Epoxy Resin PERMABOND® ES562 is a single-part epoxy adhesive which flows like solder when heated during curing. The adhesive has excellent adhesion to metal surfaces and composites. The high bond strength of t.. |
|||
Adhesive Bond Strength | 14.0 - 27.0 MPa | 2030 - 3920 psi | Zinc, Shear; ISO 4587 |
Permabond ES562 Epoxy Resin PERMABOND® ES562 is a single-part epoxy adhesive which flows like solder when heated during curing. The adhesive has excellent adhesion to metal surfaces and composites. The high bond strength of t.. |
|||
Adhesive Bond Strength | 14.0 - 27.0 MPa | 2030 - 3920 psi | Zinc, Shear; ASTM D1002 |
Permabond ES578 Epoxy Resin PERMABOND® ES578 is a single-part heat cured epoxy adhesive with excellent adhesion to metal surfaces, ceramics as well as composite materials. ES578 provides excellent thermal conductivity and bon.. |
|||
Adhesive Bond Strength | 14.0 - 27.0 MPa | 2030 - 3920 psi | Zinc, Shear; ASTM D1002 |
Permabond ES569 Epoxy Resin PERMABOND® ES569 is a single-part heat cured epoxy adhesive with excellent adhesion to metal surfaces as well as composite materials. The high bond strength of this adhesive allows it to replace me.. |