Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 10.0 - 11.0 MPa | 1450 - 1600 psi | Glass/steel, Shear |
Permabond UV625 UV-curable Adhesive PERMABOND UV625 is a single part, fast curing, UV curable adhesive primarily designed for bonding and sealing glass and metal. The cured adhesive is tough, flexible and has excellent impact resistan.. |
|||
Adhesive Bond Strength | 9.00 - 11.0 MPa | 1310 - 1600 psi | FRP Glass/Epoxy, Shear; ASTM D1002 |
Permabond ES569 Epoxy Resin PERMABOND® ES569 is a single-part heat cured epoxy adhesive with excellent adhesion to metal surfaces as well as composite materials. The high bond strength of this adhesive allows it to replace me.. |