Mechanical Properties Metric English Comments
Adhesive Bond Strength >= 6.00 MPa
>= 870 psi
ABS, Substrate Failure, Shear; ISO 4587
Permabond 101 Cyanoacrylate, Wicking Viscosity
PERMABOND® 101 is a low viscosity product useful in wicking or penetrating applications or bonding closely fitting parts. It is fast setting and suitable for use on plastics, rubber and metals. Cya..
Adhesive Bond Strength >= 6.00 MPa
>= 870 psi
PVC, Substrate Failure, Shear; ISO 4587
Permabond 101 Cyanoacrylate, Wicking Viscosity
PERMABOND® 101 is a low viscosity product useful in wicking or penetrating applications or bonding closely fitting parts. It is fast setting and suitable for use on plastics, rubber and metals. Cya..
Adhesive Bond Strength >= 6.00 MPa
>= 870 psi
ABS, Substrate Failure, Shear; ISO 4587
Permabond 105 Cyanoacrylate, for difficult rubbers
PERMABOND® 105 is a low viscosity high purity cyanoacrylate adhesive. It is ideal for use on hard-to-bond plastics and rubbers such as natural rubber, EPDM and butyl rubber. Cyanoacrylate adhesives..
Adhesive Bond Strength >= 6.00 MPa
>= 870 psi
PVC, Substrate Failure, Shear; ISO 4587
Permabond 105 Cyanoacrylate, for difficult rubbers
PERMABOND® 105 is a low viscosity high purity cyanoacrylate adhesive. It is ideal for use on hard-to-bond plastics and rubbers such as natural rubber, EPDM and butyl rubber. Cyanoacrylate adhesives..
Adhesive Bond Strength 6.00 - 8.00 MPa
870 - 1160 psi
Aluminum, Shear; ISO 4587
Permabond 105 Cyanoacrylate, for difficult rubbers
PERMABOND® 105 is a low viscosity high purity cyanoacrylate adhesive. It is ideal for use on hard-to-bond plastics and rubbers such as natural rubber, EPDM and butyl rubber. Cyanoacrylate adhesives..
Adhesive Bond Strength 6.00 - 8.00 MPa
870 - 1160 psi
Zinc, Shear; ISO 4587
Permabond 105 Cyanoacrylate, for difficult rubbers
PERMABOND® 105 is a low viscosity high purity cyanoacrylate adhesive. It is ideal for use on hard-to-bond plastics and rubbers such as natural rubber, EPDM and butyl rubber. Cyanoacrylate adhesives..
Adhesive Bond Strength >= 6.00 MPa
>= 870 psi
PVC, Substrate Failure, Shear; ISO 4587
Permabond 2010 Cyanoacrylate, gap filling
PERMABOND 200 is a high viscosity product with good flow control useful in wire tacking applications or bonding components. It is fast setting and suitable for use on plastics, rubber and metals. Cy..
Adhesive Bond Strength >= 6.00 MPa
>= 870 psi
ABS, Substrate Failure, Shear; ISO 4587
Permabond 2010 Cyanoacrylate, gap filling
PERMABOND 200 is a high viscosity product with good flow control useful in wire tacking applications or bonding components. It is fast setting and suitable for use on plastics, rubber and metals. Cy..
Adhesive Bond Strength >= 6.00 MPa
>= 870 psi
ABS, Substrate Failure, Shear; ISO 4587
Permabond 2011 Cyanoacrylate, gel
PERMABOND® 2011 is a thixotropic, fast-setting cyanoacrylate particularly suitable for use on vertical and porous substrates. This material can be used on metals, plastics, elastomers, ceramics and..
Adhesive Bond Strength >= 6.00 MPa
>= 870 psi
PVC, Substrate Failure, Shear; ISO 4587
Permabond 2011 Cyanoacrylate, gel
PERMABOND® 2011 is a thixotropic, fast-setting cyanoacrylate particularly suitable for use on vertical and porous substrates. This material can be used on metals, plastics, elastomers, ceramics and..
Adhesive Bond Strength >= 6.00 MPa
>= 870 psi
ABS, Substrate Failure, Shear; ISO 4587
Permabond 2050 Cyanoacrylate, flexible
PERMABOND® 2050 is a flexible cyanoacrylate adhesive, exhibiting improved peel strengths when compared to other grades. It has excellent impact and vibration resistance, and is suitable for bonding..
Adhesive Bond Strength >= 6.00 MPa
>= 870 psi
PVC, Substrate Failure, Shear; ISO 4587
Permabond 2050 Cyanoacrylate, flexible
PERMABOND® 2050 is a flexible cyanoacrylate adhesive, exhibiting improved peel strengths when compared to other grades. It has excellent impact and vibration resistance, and is suitable for bonding..
Adhesive Bond Strength >= 6.00 MPa
>= 870 psi
ABS, Substrate Failure, Shear; ISO 4587
Permabond 735 Cyanoacrylate, toughened
PERMABOND® 735 is a toughened cyanoacrylate with very good impact and peel strength when compared to a conventional cyanoacrylate. It bonds rapidly at room temperature and its viscosity is stable o..
Adhesive Bond Strength >= 6.00 MPa
>= 870 psi
PVC, Substrate Failure, Shear; ISO 4587
Permabond 735 Cyanoacrylate, toughened
PERMABOND® 735 is a toughened cyanoacrylate with very good impact and peel strength when compared to a conventional cyanoacrylate. It bonds rapidly at room temperature and its viscosity is stable o..
Adhesive Bond Strength >= 6.00 MPa
>= 870 psi
ABS, Substrate Failure, Shear; ISO 4587
Permabond 737 Cyanoacrylate, toughened
PERMABOND® 737 is a toughened cyanoacrylate with improved impact and peel strength for maximum flexibility. Its increased temperature resistance and dark color make 737 suitable for a wide range of..
Adhesive Bond Strength >= 6.00 MPa
>= 870 psi
PVC, Substrate Failure, Shear; ISO 4587
Permabond 737 Cyanoacrylate, toughened
PERMABOND® 737 is a toughened cyanoacrylate with improved impact and peel strength for maximum flexibility. Its increased temperature resistance and dark color make 737 suitable for a wide range of..
Adhesive Bond Strength >= 6.00 MPa
>= 870 psi
ABS, Substrate Failure, Shear; ISO 4587
Permabond 940 Cyanoacrylate, low odor
PERMABOND 940 is a low odor, non-fogging non-frosting alkoxyethyl cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate ad..
Adhesive Bond Strength 6.00 - 8.00 MPa
870 - 1160 psi
FRP Glass Polyester, Shear; ISO 4587
Permabond ET5401 Epoxy Resin
PERMABOND® ET5401 is a two-part, 2:1 mixable, semi-flexible toughened no slump epoxy adhesive with good adhesion to a variety of substrates such as wood, metal, ceramics and some plastics and compo..
Adhesive Bond Strength 6.00 MPa
870 psi
steel collar and pin shear; ISO 10123
Permabond HH190 Anaerobic Gasketmaker
Permabond® HH190 Gasketmaker is an anaerobic curing flange sealant that can replace, or be used as a dressing for, conventional pre-cut gaskets. Since HH190 is a flowable paste, it conforms to the ..
Adhesive Bond Strength >= 6.00 MPa
>= 870 psi
ABS, Substrate Failure, Shear
Permabond 102 Cyanoacrylate, General purpose
PERMABOND® 102 is a low viscosity general purpose cyanoacrylate adhesive suitable for bonding close-fitting components. It is fast setting and suitable for use on plastics, rubber and metals. Cyano..
Adhesive Bond Strength >= 6.00 MPa
>= 870 psi
PVC, Substrate Failure, Shear
Permabond 102 Cyanoacrylate, General purpose
PERMABOND® 102 is a low viscosity general purpose cyanoacrylate adhesive suitable for bonding close-fitting components. It is fast setting and suitable for use on plastics, rubber and metals. Cyano..
Adhesive Bond Strength >= 6.00 MPa
>= 870 psi
ABS, Substrate Failure, Shear; ISO 4587
Permabond 240 Cyanoacrylate, gap filling
PERMABOND® 240 is a high viscosity product useful in large gap applications. It is ideal for porous substrates. It is fast setting and suitable for use on plastics, rubber and metals. Cyanoacrylate..
Adhesive Bond Strength >= 6.00 MPa
>= 870 psi
PVC, Substrate Failure, Shear; ISO 4587
Permabond 240 Cyanoacrylate, gap filling
PERMABOND® 240 is a high viscosity product useful in large gap applications. It is ideal for porous substrates. It is fast setting and suitable for use on plastics, rubber and metals. Cyanoacrylate..
Adhesive Bond Strength >= 6.00 MPa
>= 870 psi
PVC, Substrate Failure, Shear; ISO 4587
Permabond 920 Cyanoacrylate, High temperature
PERMABOND® 920 is the original allyl cyanoacrylate adhesive. It is a single part, low viscosity liquid that will cure rapidly at room temperature when pressed into a thin film between parts. PERMAB..
Adhesive Bond Strength >= 6.00 MPa
>= 870 psi
ABS, Substrate Failure, Shear; ISO 4587
Permabond 920 Cyanoacrylate, High temperature
PERMABOND® 920 is the original allyl cyanoacrylate adhesive. It is a single part, low viscosity liquid that will cure rapidly at room temperature when pressed into a thin film between parts. PERMAB..
Adhesive Bond Strength >= 6.00 MPa
>= 870 psi
ABS, Substrate Failure, Shear; ISO 4587
Permabond 941 Cyanoacrylate, low odor
PERMABOND 941 is a low odor, non-fogging non-frosting alkoxyethyl cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate ad..
Adhesive Bond Strength >= 6.00 MPa
>= 870 psi
ABS, Substrate Failure, Shear; ISO 4587
Permabond 943 Cyanoacrylate, low odor
PERMABOND 943 is a low odor, non-fogging non-frosting alkoxyethyl cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate ad..
Adhesive Bond Strength >= 6.00 MPa
>= 870 psi
ABS, Substrate Failure, Shear; ISO 4587
Permabond 947 Cyanoacrylate, low odor
PERMABOND 947 is a low odor, non-fogging non-frosting alkoxyethyl cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate ad..
Adhesive Bond Strength 6.00 MPa
870 psi
steel collar and pin shear; ISO 10123
Permabond A131 Anaerobic Threadsealant
Permabond® A131 is an anaerobic adhesive designed to seal threaded metal pipe connections carrying a wide variety of gases and liquids, including potable water. Suitable for use on both parallel an..