Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 36.2 MPa | 5250 psi | Steel-Steel; after optimum cure |
Armstrong C-4/W Epoxy Adhesive A low viscosity, clear amber, unfilled adhesive, recommended for use with activators D or W. C-4 with Activator W offers maximum versatility in that differing degrees of flexibility can be achieved .. |