Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 29.6 MPa | 4300 psi | Steel lap shear |
Resinlab® CYNERGY CA6003 Adhesive Description: The CYNERGY 6000 SERIES are for use in demanding applications where very fast cure speeds are required. These are single component solvent free materials manufactured in a wide variety.. |
|||
Adhesive Bond Strength | 29.6 MPa | 4300 psi | Steel lap shear |
Resinlab® CYNERGY CA6005 Adhesive Description: The CYNERGY 6000 SERIES are for use in demanding applications where very fast cure speeds are required. These are single component solvent free materials manufactured in a wide variety.. |
|||
Adhesive Bond Strength | 29.6 MPa | 4300 psi | Steel lap shear |
Resinlab® CYNERGY CA6006 Adhesive Description: The CYNERGY 6000 SERIES are for use in demanding applications where very fast cure speeds are required. These are single component solvent free materials manufactured in a wide variety.. |
|||
Adhesive Bond Strength | 29.6 MPa | 4300 psi | Steel lap shear |
Resinlab® CYNERGY CA6007 Adhesive Description: The CYNERGY 6000 SERIES are for use in demanding applications where very fast cure speeds are required. These are single component solvent free materials manufactured in a wide variety.. |
|||
Adhesive Bond Strength | 29.6 MPa | 4300 psi | Steel lap shear |
Resinlab® CYNERGY CA6008 Adhesive Description: The CYNERGY 6000 SERIES are for use in demanding applications where very fast cure speeds are required. These are single component solvent free materials manufactured in a wide variety.. |
|||
Adhesive Bond Strength | 29.6 MPa | 4300 psi | Steel lap shear |
Resinlab® CYNERGY CA6009 Adhesive Description: The CYNERGY 6000 SERIES are for use in demanding applications where very fast cure speeds are required. These are single component solvent free materials manufactured in a wide variety.. |
|||
Adhesive Bond Strength | 29.6 MPa | 4300 psi | Steel lap shear |
Resinlab® CYNERGY CA6010 Adhesive Description: The CYNERGY 6000 SERIES are for use in demanding applications where very fast cure speeds are required. These are single component solvent free materials manufactured in a wide variety.. |
|||
Adhesive Bond Strength | 29.6 MPa | 4300 psi | Steel lap shear |
Resinlab® CYNERGY CA6011 Adhesive Description: The CYNERGY 6000 SERIES are for use in demanding applications where very fast cure speeds are required. These are single component solvent free materials manufactured in a wide variety.. |
|||
Adhesive Bond Strength | 29.6 MPa | 4300 psi | Steel lap shear |
Resinlab® CYNERGY CA6012 Adhesive Description: The CYNERGY 6000 SERIES are for use in demanding applications where very fast cure speeds are required. These are single component solvent free materials manufactured in a wide variety.. |
|||
Adhesive Bond Strength | 29.6 MPa | 4300 psi | Steel lap shear |
Resinlab® CYNERGY CA6013 Adhesive Description: The CYNERGY 6000 SERIES are for use in demanding applications where very fast cure speeds are required. These are single component solvent free materials manufactured in a wide variety.. |
|||
Adhesive Bond Strength | 29.6 MPa | 4300 psi | Steel lap shear |
Resinlab® CYNERGY CA6014 Adhesive Description: The CYNERGY 6000 SERIES are for use in demanding applications where very fast cure speeds are required. These are single component solvent free materials manufactured in a wide variety.. |
|||
Adhesive Bond Strength | 29.6 MPa | 4300 psi | Steel lap shear |
Resinlab® CYNERGY CA6015 Adhesive Description: The CYNERGY 6000 SERIES are for use in demanding applications where very fast cure speeds are required. These are single component solvent free materials manufactured in a wide variety.. |
|||
Adhesive Bond Strength | 29.6 MPa | 4300 psi | Steel lap shear |
Resinlab® CYNERGY CA6809 Adhesive Description: The CYNERGY 6800 SERIES are clear, high strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. This series of products has USP .. |
|||
Adhesive Bond Strength | 29.6 MPa | 4300 psi | Steel lap shear |
Resinlab® CYNERGY CA6813 Adhesive Description: The CYNERGY 6800 SERIES are clear, high strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. This series of products has USP .. |
|||
Adhesive Bond Strength | 29.6 MPa | 4300 psi | Steel lap shear |
Resinlab® CYNERGY CA6001 Adhesive Description: The CYNERGY 6000 SERIES are for use in demanding applications where very fast cure speeds are required. These are single component solvent free materials manufactured in a wide variety.. |
|||
Adhesive Bond Strength | 29.6 MPa | 4300 psi | Steel lap shear |
Resinlab® CYNERGY CA6002 Adhesive Description: The CYNERGY 6000 SERIES are for use in demanding applications where very fast cure speeds are required. These are single component solvent free materials manufactured in a wide variety.. |
|||
Adhesive Bond Strength | 29.6 MPa | 4300 psi | Steel lap shear |
Resinlab® CYNERGY CA6004 Adhesive Description: The CYNERGY 6000 SERIES are for use in demanding applications where very fast cure speeds are required. These are single component solvent free materials manufactured in a wide variety.. |
|||
Adhesive Bond Strength | 29.6 MPa | 4300 psi | Steel lap shear |
Resinlab® CYNERGY CA6801 Adhesive Description: The CYNERGY 6800 SERIES are clear, high strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. This series of products has USP .. |
|||
Adhesive Bond Strength | 29.6 MPa | 4300 psi | Steel lap shear |
Resinlab® CYNERGY CA6802 Adhesive Description: The CYNERGY 6800 SERIES are clear, high strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. This series of products has USP .. |
|||
Adhesive Bond Strength | 29.6 MPa | 4300 psi | Steel lap shear |
Resinlab® CYNERGY CA6803 Adhesive Description: The CYNERGY 6800 SERIES are clear, high strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. This series of products has USP .. |
|||
Adhesive Bond Strength | 29.6 MPa | 4300 psi | Steel lap shear |
Resinlab® CYNERGY CA6804 Adhesive Description: The CYNERGY 6800 SERIES are clear, high strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. This series of products has USP .. |
|||
Adhesive Bond Strength | 29.6 MPa | 4300 psi | Steel lap shear |
Resinlab® CYNERGY CA6805 Adhesive Description: The CYNERGY 6800 SERIES are clear, high strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. This series of products has USP .. |
|||
Adhesive Bond Strength | 29.6 MPa | 4300 psi | Steel lap shear |
Resinlab® CYNERGY CA6806 Adhesive Description: The CYNERGY 6800 SERIES are clear, high strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. This series of products has USP .. |
|||
Adhesive Bond Strength | 29.6 MPa | 4300 psi | Steel lap shear |
Resinlab® CYNERGY CA6807 Adhesive Description: The CYNERGY 6800 SERIES are clear, high strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. This series of products has USP .. |
|||
Adhesive Bond Strength | 29.6 MPa | 4300 psi | Steel lap shear |
Resinlab® CYNERGY CA6808 Adhesive Description: The CYNERGY 6800 SERIES are clear, high strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. This series of products has USP .. |
|||
Adhesive Bond Strength | 29.6 MPa | 4300 psi | Steel lap shear |
Resinlab® CYNERGY CA6810 Adhesive Description: The CYNERGY 6800 SERIES are clear, high strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. This series of products has USP .. |
|||
Adhesive Bond Strength | 29.6 MPa | 4300 psi | Steel lap shear |
Resinlab® CYNERGY CA6811 Adhesive Description: The CYNERGY 6800 SERIES are clear, high strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. This series of products has USP .. |
|||
Adhesive Bond Strength | 29.6 MPa | 4300 psi | Steel lap shear |
Resinlab® CYNERGY CA6812 Adhesive Description: The CYNERGY 6800 SERIES are clear, high strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. This series of products has USP .. |
|||
Adhesive Bond Strength | 29.6 MPa | 4300 psi | Lap shear, alum to alum, 15 min @ 90°C |
Tra-Con Tra-Bond F112 Fiber Optic Epoxy Adhesive TRA-BOND F112 is a long pot life, impact resistant, fiber-optic adhesive. This two-part, low viscosity epoxy has the distinct advantage of remaining below 3000 cps for a minimum of 40 minutes. This .. |
|||
Adhesive Bond Strength | 29.6 MPa | 4300 psi | Lap shear, alum to alum, 4 hrs @ 65°C |
Tra-Con Tra-Bond 216C04 Information provided by Tra-Con Inc. |