Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 18.6 MPa | 2700 psi | Lap shear; 2024 T3 Al Abraded / MEK Wipe |
Resinlab® EP1285HD-16 Highly Filled, Medium Viscosity Casting Resin Resinlab™ EP1285 (Formerly Lab Product W021901 series) is a highly filled, medium viscosity black casting resin designed for applications requiring a high degree of thermal conductivity and a low C.. |
|||
Adhesive Bond Strength | 18.6 MPa | 2700 psi | Grit Blasted Steel, Shear; ASTM D1002 |
Permabond 930 Cyanoacrylate PERMABOND 930 is a low odor, nonfogging, nonfrosting cyanoacrylate. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate adhesives on hot and humid days, is eliminated. The .. |
|||
Adhesive Bond Strength | 18.6 MPa | 2700 psi | Grit Blasted Steel, Shear; ASTM D1002 |
Permabond 931 Cyanoacrylate PERMABOND 931 is a low odor, nonfogging, nonfrosting cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate adhesiv.. |
|||
Adhesive Bond Strength | 18.6 MPa | 2700 psi | Grit Blasted Steel, Shear; ASTM D1002 |
Permabond 932 Cyanoacrylate PERMABOND 932 is a low odor, nonfogging, nonfrosting cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate adhesiv.. |
|||
Adhesive Bond Strength | 18.6 MPa | 2700 psi | Lap shear, alum to alum, 2 hrs @ 65°C |
Tra-Con Tra-Bond 2126 Black Opaque Epoxy Adhesive TRA-BOND 2126 is recommended for those modern photographic, industrial, and laboratory bonding and laminating applications where an easy-to-use, black (opaque) epoxy adhesive system with high perfor.. |
|||
Adhesive Bond Strength | 18.6 MPa | 2700 psi | Lap shear, alum to alum, 24 hrs @ 25°C |
Tra-Con Tra-Bond F113SC High Tg Fiber Optic Epoxy Adhesive TRA-BOND F113SC is a room temperature curing, high Tg and low viscosity adhesive formulated for terminating ALL TYPES of fiber optic connectors. It has also been used for bonding LED displays, lense.. |
|||
Adhesive Bond Strength | 18.6 MPa | 2700 psi | Lap shear, alum to alum |
Tra-Con Tra-Bond F253 Color Keyed High Temperature Epoxy Adhesive TRA-BOND F253 is a low viscosity, high temperature, two-part epoxy formulation that changes color during the curing process to indicate cure status. The unmixed components are light yellow; the mixt.. |
|||
Adhesive Bond Strength | 18.6 MPa | 2700 psi | Lap shear, alum to alum, 4 hrs @ 65°C |
Tra-Con Tra-Bond FS469 Clear High Strength Epoxy TRA-BOND FS469 is a clear low viscosity epoxy formulation designed for bonding and coating micro-electronics, laminations, optical components and laser assemblies. The low cure shrinkage (using a ro.. |
|||
Adhesive Bond Strength | >= 18.6 MPa | >= 2700 psi | |
Master Bond EP41SMed Two Component, Low Viscosity, USP Class VI Epoxy System Master Bond Polymer Adhesive EP41S Medical is a two component low viscosity epoxy resin system for high performance bonding, sealing, coating, as well as small encapsulations, pottings and castings... |
|||
Adhesive Bond Strength | 18.6 MPa | 2700 psi | Lap shear, alum to alum, cured 10 min @ 140°C |
Tra-Con Tra-Bond 526M05 Rapid Low Temperature Cure Adhesive TRA-BOND 526M05 is a low viscosity, fast cure at low temperature, long pot-life adhesive. Information provided by Tra-Con Inc. |
|||
Adhesive Bond Strength | 18.6 MPa | 2700 psi | Lap shear, alum to alum |
Tra-Con Tra-Bond 9426M Epoxy Adhesive TRA-BOND 9426M is an epoxy adhesive formulated to provide tough resilient bonds and excellent adhesion to a wide variety of substrates including metals, glass, ceramics, wood and many plastics. Info.. |
|||
Adhesive Bond Strength | 18.6 MPa | 2700 psi | Varies with substrates |
Loctite® SpeedBonder™ 326 Fast Fixture Acrylic Bonding Adhesive Acrylic Bonding AdhesivesLoctite® Acrylic Adhesives were developed for bonding applications that require tensile, shear and peel strength combined with maximum impact, stress and shock resistance. .. |
|||
Adhesive Bond Strength | 18.6 MPa | 2700 psi | adhesion to Saran™ film after 3 days at 72°F; ASTM D3330 |
Dow Saran® 520 Vapor Retarder Tape Saran™ 520 Vapor Retarder Tape is a Vapor Retarder Film coated with acrylic adhesive designed for long-lasting adhesion and wide temperature range performance. Information provided by Dow |