Polymer Property : Adhesive Bond Strength = 16.38 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Adhesive Bond Strength 16.38 MPa
2375 psi
Adhesive tensile shear strength; ASTM D1002
Devcon Combo Wear FC Epoxy
Abrasion-Resistant SystemComments: PuttyData provided by Ellsworth Adhesives.
Adhesive Bond Strength 16.38 MPa
2375 psi
Adhesive tensile shear strength; ASTM D1002
Devcon Wear Guard (Fine Load) Epoxy
Abrasion-Resistant SystemComments: PuttyData provided by Ellsworth Adhesives.
Adhesive Bond Strength 16.38 MPa
2375 psi
Adhesive tensile shear strength; ASTM D1002
Devcon Wear Guard (High Load) Epoxy
Abrasion-Resistant SystemComments: PuttyData provided by Ellsworth Adhesives.