Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 150 MPa @Diameter <=100 mm |
21800 psi @Diameter <=3.94 in |
24hr/23°C/50% RH; IEC 60212-2; IEC/EN 61212-2 5.3 |
Elektro-Isola Etronax MMMF Phenolic, Cotton Fabric Reinforcement, Brown, Tubes Description: Mechanical applications. Impact-resistant, noise-reducing, wear-resistant material. Well suited as a low-friction material. High wear resistance in aggressive and dust-filled environmen.. |
|||
Adhesive Bond Strength | 150 MPa @Diameter <=100 mm |
21800 psi @Diameter <=3.94 in |
24hr/23°C/50% RH; IEC 60212-2; IEC/EN 61212-2 5.3 |
Elektro-Isola Etronit B 66 Phenolic, Paper Reinforcement, Dark Brown, Tubes Description: Specially designed for high-voltage insulation with high requirements for insulating capacity along the tube.Applications: Insulating tubes in high-voltage switchgear and tap changers.... |
|||
Adhesive Bond Strength | 150 MPa @Diameter <=100 mm |
21800 psi @Diameter <=3.94 in |
24hr/23°C/50% RH; IEC 60212-2; IEC/EN 61212-2 5.3 |
Elektro-Isola G-Etronax SI Silicone, Glass Fabric Reinforcement, White, Tubes Description: Used in mechanical, electrical and electronic applications at elevated temperatures. Retains good electrical properties at high temperatures. Self-extinguishing. Low dielectric loss fac.. |
|||
Adhesive Bond Strength | 150 MPa @Diameter <=100 mm |
21800 psi @Diameter <=3.94 in |
24hr/23°C/50% RH; IEC 60212-2; IEC/EN 61212-2 5.3 |
Elektro-Isola Etronax MFP G Phenolic, Cotton Fabric Reinforcement, Black, Tubes Description: Exclusively for mechanical applications. The combination of cotton/synthetic reinforcement and a graphite-modified resin results in a material with low friction and especially high wear.. |