Polymer Property : Adhesive Bond Strength = 14.8 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Adhesive Bond Strength 14.8 MPa
2150 psi
Lap shear, alum to alum, 24 hrs @ 25°C
Tra-Con Tra-Bond F110 Optically Transparent Low Viscosity Epoxy Adhesive
TRA-BOND F110 is a rigid, optically clear adhesive with a very low viscosity. This room temperature curing system is an excellent choice for thin bond-line assembly and repair applications of prisms..
Adhesive Bond Strength 14.8 MPa

@Temperature 82.2 °C
2150 psi

@Temperature 180 °F
Aluminum-Aluminum tensile shear
Armstrong A-12-T Epoxy Adhesive
Provides the same basic properties as A-12, but in thixotropic, non-sag, easily-brushable paste form. An ideal material for use where adhesive flow during cure cannot be tolerated. A-12-T meets t..
Adhesive Bond Strength 14.8 MPa

@Temperature -54.4 °C
2150 psi

@Temperature -66.0 °F
Aluminum-Aluminum tensile shear
Armstrong A-5/E Epoxy Adhesive
Information provided by Ellsworth Adhesives.
Adhesive Bond Strength 14.8 MPa

@Temperature 25.0 °C
2150 psi

@Temperature 77.0 °F
Aluminum-Aluminum tensile shear
Armstrong A-702 Epoxy Adhesive
Information provided by Ellsworth Adhesives.
Adhesive Bond Strength 14.8 MPa

@Temperature 82.2 °C
2150 psi

@Temperature 180 °F
Aluminum-Aluminum tensile shear
Armstrong C-1/A Epoxy Adhesive
A versatile, low viscosity, unfilled resin used for electrical potting and laminating applications. It is an excellent insulator, and provides outstanding chemical resistance to most compoundsInfor..