Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 12.0 - 14.0 MPa | 1740 - 2030 psi | Phenolic, Shear; ISO 4587 |
Permabond 101 Cyanoacrylate, Wicking Viscosity PERMABOND® 101 is a low viscosity product useful in wicking or penetrating applications or bonding closely fitting parts. It is fast setting and suitable for use on plastics, rubber and metals. Cya.. |
|||
Adhesive Bond Strength | 12.0 - 14.0 MPa | 1740 - 2030 psi | Phenolic, Shear; ISO 4587 |
Permabond 105 Cyanoacrylate, for difficult rubbers PERMABOND® 105 is a low viscosity high purity cyanoacrylate adhesive. It is ideal for use on hard-to-bond plastics and rubbers such as natural rubber, EPDM and butyl rubber. Cyanoacrylate adhesives.. |
|||
Adhesive Bond Strength | 12.0 - 14.0 MPa | 1740 - 2030 psi | Mild steel, Shear |
Permabond ET500 Epoxy Resin PERMABOND ET500 is a two-part fast-setting epoxy adhesive which bonds to a wide variety of substrates such as wood, metal, ceramics and some plastics and composites. It cures rapidly at room tempera.. |
|||
Adhesive Bond Strength | 12.0 - 18.0 MPa | 1740 - 2610 psi | Zinc, Shear |
Permabond TA439 Toughened Acrylic Adhesive Permabond® TA439 is a two component structural acrylic adhesive designed primarily for bonding metals, ferrites, ceramics and some plastics. The typical fixture time of is 10-30 seconds. The fast f.. |
|||
Adhesive Bond Strength | 12.0 - 18.0 MPa | 1740 - 2610 psi | Zinc Plated after 24 hours, Shear |
Permabond TA459 Toughened Acrylic Adhesive Permabond TA459 is a structural acrylic adhesive designed primarily for bonding metals, ferrites, ceramics and some thermoplastics. This product was specifically designed to be non-corrosive to sens.. |
|||
Adhesive Bond Strength | 12.0 - 18.0 MPa | 1740 - 2610 psi | Zinc Plated after 24 hours, Shear |
Permabond TA4590 Toughened Acrylic Adhesive Permabond TA4590 is a structural acrylic adhesive designed primarily for bonding metals, ferrites, ceramics and some thermoplastics. This product was specifically designed to be non-corrosive to sen.. |
|||
Adhesive Bond Strength | 12.0 - 14.0 MPa | 1740 - 2030 psi | Phenolic, Shear |
Permabond 102 Cyanoacrylate, General purpose PERMABOND® 102 is a low viscosity general purpose cyanoacrylate adhesive suitable for bonding close-fitting components. It is fast setting and suitable for use on plastics, rubber and metals. Cyano.. |
|||
Adhesive Bond Strength | 12.0 MPa | 1740 psi | Lap Shear Cohesive Strength; ASTM D1002 |
ITW Plexus Plexusâ„¢ 3940 Methacrylate Adhesive An adhesive with versatile substrate and application capabilities for a wide range of industrial product assembly applications.Fast tacking, low pressure sprayable adhesive with long bonding range, .. |
|||
Adhesive Bond Strength | 12.0 MPa | 1740 psi | steel collar and pin shear; ISO 10123 |
Permabond A1042 Anaerobic Threadlocker Permabond® A1042 is a rapid curing adhesive designed to lock and seal metal parts that subsequently may need to be dismantled for maintenance. The high vibration resistance makes Permabond A1042 pa.. |
|||
Adhesive Bond Strength | 12.0 MPa | 1740 psi | Tensile shear per ASTM D1002 on etched Al panel |
Von Roll Isola IMI E-Solder® 3083 Electrically Conductive Adhesive Data provided by Von Roll Isola USA.E-SOLDER® epoxy based resin systems can be used at room temperature on heat sensitive materials, can bond dissimilar materials, and do not have flux or residue t.. |
|||
Adhesive Bond Strength | 12.0 MPa | 1740 psi | steel collar and pin shear; ISO 10123 |
Permabond A113 Anaerobic Threadlocker Designed for the locking and sealing of metal parts, Permabond® A113 is ideally suited for use on components that need to be dismantled for maintenance. Giving vibration resistance it can be used .. |
|||
Adhesive Bond Strength | 12.0 MPa | 1740 psi | steel collar and pin shear; ISO 10123 |
Permabond A130 Anaerobic Threadlocker Designed for the locking and sealing of metal parts, Permabond® A130 is ideally suited for use on components that need to be dismantled for maintenance. Giving vibration resistance it can be used t.. |
|||
Adhesive Bond Strength | 12.0 MPa | 1740 psi | steel collar and pin shear; ISO 10123 |
Permabond A136 Anaerobic Gasketmaker Permabond® A136 is an anaerobic material designed for making 'formed in situ' gaskets between metal surfaces. It is capable of replacing a wide range of conventional gaskets thereby offering potent.. |