Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 0.600 - 29.0 MPa | 87.0 - 4200 psi | Average value: 19.5 MPa Grade Count:23 |
Overview of materials for Methacrylate Adhesive This property data is a summary of similar materials in the MatWeb database for the category "Methacrylate Adhesive". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Adhesive Bond Strength | 0.600 MPa | 87.0 psi | Peel Strength to Polycarbonate Alloy (Cohesive Failure), ASTM D1876 |
ITW Plexus Plexusâ„¢ MA200 Methacrylate Adhesive Two component adhesive that expands to twice original volume without toxic blowing agents. Used where weight, gap-filling, or increased toughness (vibration damping) is requires for the bonded join.. |