Mechanical Properties | Metric | English | Comments |
---|---|---|---|
2% Secant Modulus | 0.172 GPa | 24.9 ksi | 12.7mm/min; ASTM D790 |
Westlake EC811AA Low Density Polyethylene WESTLAKE low-density polyethylene EC811 is used for extrusion coating applications. It exhibits good adhesion, low coat weight, and fast heat seals.Application/UsesCoatings for paper/paperboardFDA: .. |
|||
2% Secant Modulus | 0.172 GPa | 24.9 ksi | 12.7mm/min; ASTM D790 |
Westlake EC850AA Low Density Polyethylene WESTLAKE low-density polyethylene EC850 is a resin designed for applications where high coating speeds and good drawdown are required. The combination of high melt index and low density provides goo.. |