Mechanical Properties | Metric | English | Comments |
---|---|---|---|
2% Secant Modulus | 0.9018 GPa | 130.8 ksi | 12.5mm/min; ASTM D790 |
LyondellBasell Alathon® H4262 High Density Polyethylene, Injection Molding Grade
(discontinued **) ApplicationsAlathon H4262 is a high-flow resin that exhibits very good cold temperature impact performance, optimum processing and thermal stability, with good color and organoleptic properties. Typ.. |