Mechanical Properties | Metric | English | Comments |
---|---|---|---|
2% Secant Modulus | 0.00690 GPa | 1.00 ksi | ASTM D790 |
Dow Engage® 8130 Polyolefin Elastomer Description: Engage® 8130 polyolefin elastomer is an ethyleneoctene copolymer with low density and a high melt index. This combination provides excellent toughness, flexibility, and ease in process.. |