Polymer Property : 2% Secant Modulus = 0.172 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
2% Secant Modulus 0.172 GPa
24.9 ksi
12.7mm/min; ASTM D790
Westlake EC811AA Low Density Polyethylene
WESTLAKE low-density polyethylene EC811 is used for extrusion coating applications. It exhibits good adhesion, low coat weight, and fast heat seals.Application/UsesCoatings for paper/paperboardFDA: ..
2% Secant Modulus 0.172 GPa
24.9 ksi
12.7mm/min; ASTM D790
Westlake EC850AA Low Density Polyethylene
WESTLAKE low-density polyethylene EC850 is a resin designed for applications where high coating speeds and good drawdown are required. The combination of high melt index and low density provides goo..