Mechanical Properties | Metric | English | Comments |
---|---|---|---|
2% Secant Modulus | 0.0110 GPa | 1.60 ksi | ASTM D790 |
Dow Engage® ENR 8556.00 Ethylene-Octene Copolymer Description: ENR 8556.00 polyolefin elastomer is an ethyleneoctene copolymer that offers excellent performance in extrusion applications such as tubing and profiles. This elastomer provides excellen.. |