Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact | >= 95.0 J | >= 70.1 ft-lb | |
Industeel URANUS® 52N+ 25 Cr Super Duplex Stainless Steel with PREN = 40 Description: URANUS® 52N+ (UR 52N+) is a super duplex stainless steel with 25% Cr and a PREN value higher than 40. The minimum guaranteed yield strength is 550 MPa which allows the designer to re.. |
|||
Charpy Impact | >= 95.0 J | >= 70.1 ft-lb | |
Industeel URANUS® 47N+ 25 Cr Super Duplex Stainless Steel with PREN = 40 Description: CLI - SAF 2507® is a 25.07 super duplex stainless steel with 25% Cr and a PREN value higher than 40. The minimum guaranteed yield strength is 550 MPa which allows the designer to red.. |
|||
Charpy Impact | 95.0 J | 70.1 ft-lb | Austenitizing Temperature- 1065°C |
Crucible Steel CPM® 3V® Tool Steel CPM 3V is a new tool steel made by the Crucible Particle Metallurgy process, designed to provide maximum resistance to breakage and chipping in a highly wear-resistant steel. CPM 3V offers impact to.. |
|||
Charpy Impact | 95.0 J | 70.1 ft-lb | V-notch |
Carpenter Custom 455® Stainless Steel, Annealed, 25 mm Bar Data provided by Carpenter Technology Corporation.Recognizing the need for high-strength alloys with good corrosion resistance to atmospheric environments, the Carpenter Research Laboratory develope.. |