Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact | 42.0 J | 31.0 ft-lb | |
Haynes 242® alloy, after 4000 hours exposure at 650°C (1200°F) Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm.. |
|||
Charpy Impact | 42.0 J | 31.0 ft-lb | 50% cold rolled |
Haynes Hastelloy® G-30® alloy, 50% cold rolled HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid.. |
|||
Charpy Impact | 42.0 J | 31.0 ft-lb | aged 8000 hours at 650°C (1200°F) |
Haynes HR-160® alloy plate, aged 8000 hours at 649°C (1200°F) Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an.. |