Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact | 39.0 J | 28.8 ft-lb | |
Haynes 230® alloy plate, 4000 hours exposure at 649°C (1200°F) Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic.. |
|||
Charpy Impact | 39.0 J @Temperature 100 °C |
28.8 ft-lb @Temperature 212 °F |
V-notch. Short transverse direction. 50 HRC |
Assab Steels DIEVAR Hot Work Steel DIEVAR is a high performance chromium-molybdenum-vanadium alloyed hot work tool steel which offers a very good resistance to heat checking, gross checking, hot wear and plastic deformation. DIEVAR i.. |