Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact | 36.6 J | 27.0 ft-lb | Charpy V-notch at RT |
Kennametal Stellite Stellite® 250 Resistant to heat, thermal shock, thermal cycling, oxidation, and hot corrosion from flue gas, slags, and molten copper. Not recommended for use in abrasive wear.Applications:heat treatment furnace.. |
|||
Charpy Impact | 36.6 J @Temperature -17.7 °C |
27.0 ft-lb @Temperature 0.140 °F |
Material Condition - ST&A<sub>4</sub> |
Crucible Compaction Metals P/M 625M Corrosion Resistant Alloy P/M 625M (chemically, UNS N07626) is produced by the state-of-the-art Crucible P/M process: inert gas atomization, coupled with consolidation by hot isostatic pressing (HIP) and/or extrusion. The a.. |
|||
Charpy Impact | 36.6 J | 27.0 ft-lb | H1150-M |
Crucible Steel 17Cr-4Ni Precipitation Hardening Stainless Steel Crucible 17Cr-4Ni is a precipitation-hardening stainless steel which is capable of a high strength and hardness levels after a relatively simple heat-treatment procedure. This grade is martensitic a.. |