Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact | >= 358 J @Thickness 19.1 mm |
>= 264 ft-lb @Thickness 0.752 in |
Annealed |
Haynes Hastelloy® G-35® Nickel Alloy Plate, Annealed at 2025°F (1107°C) Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process†phosphoric acid, which is widely used in the production of fertilizers. Tests indicat.. |
|||
Charpy Impact | >= 358 J @Treatment Temp. 427 °C, Thickness 19.1 mm |
>= 264 ft-lb @Treatment Temp. 801 °F, Thickness 0.752 in |
Annealed, aged for 2000h |
Haynes Hastelloy® G-35® Nickel Alloy Plate, Annealed at 2025°F (1107°C) Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process†phosphoric acid, which is widely used in the production of fertilizers. Tests indicat.. |
|||
Charpy Impact | >= 358 J @Treatment Temp. 482 °C, Thickness 19.1 mm |
>= 264 ft-lb @Treatment Temp. 900 °F, Thickness 0.752 in |
Annealed, aged for 2000h |
Haynes Hastelloy® G-35® Nickel Alloy Plate, Annealed at 2025°F (1107°C) Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process†phosphoric acid, which is widely used in the production of fertilizers. Tests indicat.. |
|||
Charpy Impact | >= 358 J @Treatment Temp. 538 °C, Thickness 19.1 mm |
>= 264 ft-lb @Treatment Temp. 1000 °F, Thickness 0.752 in |
Annealed, aged for 2000h |
Haynes Hastelloy® G-35® Nickel Alloy Plate, Annealed at 2025°F (1107°C) Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process†phosphoric acid, which is widely used in the production of fertilizers. Tests indicat.. |
|||
Charpy Impact | >= 358 J @Treatment Temp. 593 °C, Thickness 19.1 mm |
>= 264 ft-lb @Treatment Temp. 1100 °F, Thickness 0.752 in |
Annealed, aged for 2000h |
Haynes Hastelloy® G-35® Nickel Alloy Plate, Annealed at 2025°F (1107°C) Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process†phosphoric acid, which is widely used in the production of fertilizers. Tests indicat.. |
|||
Charpy Impact | 358 J | 264 ft-lb | annealed |
Haynes HR-160® alloy, annealed plate Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an.. |
|||
Charpy Impact | 358 J | 264 ft-lb | |
Haynes Hastelloy® B-3® alloy, heat treated at 1065°C, rapid quenched The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ea.. |