Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact | 34.0 J | 25.1 ft-lb | V-notch |
Carpenter AerMet®-for-Tooling Tool Steel, Double Aged 482°C Data provided by Carpenter Technology Corporation.This is a double vacuum melted alloy with high hardness and strength combined with exceptional ductility and toughness. The alloy is designed for c.. |