Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact | 28.0 J | 20.7 ft-lb | Typical (Longitudinal) |
Industeel CLC 1.2311 Prehardened Mold Steel (300HB/30HRC) Description: CLC 1.2311 is a 300HB (30HRC) pre-hardened grade specially designed for plastic mold industry. Chromium, Molybdenum, carbon and manganese additions are optimized to have a fully martens.. |
|||
Charpy Impact | 28.0 J | 20.7 ft-lb | |
Haynes 230® alloy, plate, 8000 hours exposure at 760°C (1400°F) Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic.. |
|||
Charpy Impact | 28.0 J | 20.7 ft-lb | |
Haynes 230® alloy, plate, 8000 hours exposure at 871°C (1600°F) Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic.. |
|||
Charpy Impact | 28.0 J | 20.7 ft-lb | Austenitizing Temperature- 1010°C |
Crucible Steel AIRDI® 150 (AISI D2) Tool Steel Airdi 150 (AISI D2) is an air-hardening, high carbon, high chromium tool steel, heat treatable to HRC 60-62. It offers excellent abrasion resistance, due to a large volume of carbides in the microst.. |
|||
Charpy Impact | 28.0 J | 20.7 ft-lb | Austenitizing Temperature- 1150°C; Tempering Temperature- 580°C |
Crucible Steel Rex M2 High Speed Steel Rex M2 is a tungsten-molybdenum general purpose high speed steel. It is suitable for a wide variety of cutting tools and is often used for metalforming tools such as punches and dies. Rex M2 is a go.. |
|||
Charpy Impact | 28.0 J | 20.7 ft-lb | V notch. Short transverse direction. 700°C tempering temperature (2 + 2h). |
Assab Steels DIEVAR Hot Work Steel DIEVAR is a high performance chromium-molybdenum-vanadium alloyed hot work tool steel which offers a very good resistance to heat checking, gross checking, hot wear and plastic deformation. DIEVAR i.. |