Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact 4.00 J
2.95 ft-lb
after 8000 hours at 760°C
Haynes 188 alloy, plate at RT after 8000 hours at 760°C (1400°F)
Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr..
Charpy Impact 4.00 J

@Temperature -184 °C
2.95 ft-lb

@Temperature -299 °F
V-Notch
Carpenter Custom 455® Stainless Steel, Condition H950 (Age Hardened 510°C)
Data provided by Carpenter Technology Corporation.Recognizing the need for high-strength alloys with good corrosion resistance to atmospheric environments, the Carpenter Research Laboratory develope..