Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact | 23.0 J @Temperature -20.0 °C |
17.0 ft-lb @Temperature -4.00 °F |
Typical (Longitudinal) |
Industeel CLC 1.2311 Prehardened Mold Steel (300HB/30HRC) Description: CLC 1.2311 is a 300HB (30HRC) pre-hardened grade specially designed for plastic mold industry. Chromium, Molybdenum, carbon and manganese additions are optimized to have a fully martens.. |
|||
Charpy Impact | 23.0 J | 17.0 ft-lb | V-Notch; Air Cooled from 1010°C; 649°C Temper Temperature |
Latrobe LSSâ„¢ H12 Hot Work Tool Steel (ASTM H12) TLS H12 hot work tool steel is a 5% chromium, general-purpose hot work steel that is characterized by excellent impact toughness. It contains less vanadium than the widely-used H13 hot work tool ste.. |
|||
Charpy Impact | 23.0 J @Temperature 23.0 °C |
17.0 ft-lb @Temperature 73.4 °F |
|
Haynes Ultimet® alloy, aged 1000 hours at 871°C (1600°F) Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Charpy Impact | 23.0 J | 17.0 ft-lb | H900 |
Crucible Steel 17Cr-4Ni Precipitation Hardening Stainless Steel Crucible 17Cr-4Ni is a precipitation-hardening stainless steel which is capable of a high strength and hardness levels after a relatively simple heat-treatment procedure. This grade is martensitic a.. |
|||
Charpy Impact | 23.0 J | 17.0 ft-lb | Longitudinal |
Crucible Steel Maxel® 2000 Stainless Steel Maxel 2000 is a free-machining stainless holder block steel which is based on the nominal analysis of Type 414L rather than Type 420. It is supplied pre-hardened to about HRC 37. Due to its unique c.. |
|||
Charpy Impact | 23.0 J | 17.0 ft-lb | Austenitizing Temperature- 1190°C; Tempering Temperature- 550°C |
Crucible Steel Rex M2 High Speed Steel Rex M2 is a tungsten-molybdenum general purpose high speed steel. It is suitable for a wide variety of cutting tools and is often used for metalforming tools such as punches and dies. Rex M2 is a go.. |