Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact | 13.6 J | 10.0 ft-lb | V-Notch |
Kennametal Stellite Stellite® 21 Excellent high temperature strength, high toughness. Solution treat at 1191-1204°C, rapid air cool, age between 538-871°C to increase hardness and strength at the expense of impact and ducti.. |
|||
Charpy Impact | 13.6 - 20.3 J | 10.0 - 15.0 ft-lb | V-Notch |
Materion moldMAX® XL Spinodally Hardened Copper-Nickel-Tin Alloy moldMAX XL® is a unique spinodally hardened copper-nickel-tin alloy that combines high strength and high thermal conductivity. Available in large plate thickness up to 12†and in rounds up t.. |
|||
Charpy Impact | 13.6 - 27.1 J | 10.0 - 20.0 ft-lb | V-Notch |
Materion ToughMet® T2 CX 90 ToughMet® is Brush Wellman's solution for severe service material problems. By applying their EquaCast® process, tailored alloying additions and spinodal hardening technology, they have e.. |
|||
Charpy Impact | 13.6 J | 10.0 ft-lb | V-Notch; Air Cooled from 1024°C; 535°C Temper Temperature |
Latrobe LSSâ„¢ H13 PQ Hot Work Tool Steel TLS H13 PQ is Premium Quality H13 hot work steel that is designed to meet the highest quality standards in the die casting industry, and to excel in the most demanding hot work tooling applications... |
|||
Charpy Impact | 13.6 J | 10.0 ft-lb | V-Notch; Air Cooled from 1010°C; 535°C Temper Temperature |
Latrobe LSSâ„¢ H11 Hot Work Tool Steel (ASTM H11) TLS H11 hot work tool steel is a 5% chromium hot work steel that is characterized by excellent impact toughness. It contains less vanadium than the widely-used H13 hot work tool steel. This provides.. |
|||
Charpy Impact | 13.6 J | 10.0 ft-lb | V-Notch; 649°C Temper Temperature |
Latrobe Viscount 44® Prehardened Tool Steel (ASTM H13S) Viscount 44 is a free-machining, prehardened, H13-type hot work tool steel. It is produced using special melting, forging, and heat treating processes which provide the optimum in control
and reprod.. |
|||
Charpy Impact | 13.6 J @Temperature 23.0 °C |
10.0 ft-lb @Temperature 73.4 °F |
|
Dura-Bar 65-45-12 Continuously Cast Ductile Iron Bar Stock ASTM A536 Continuously cast ductile iron bar stock is produced in a wide variety of sizes and shapes, including rounds, rectangles and special shape cross sections.It often is used as a direct replacement for.. |
|||
Charpy Impact | 13.6 - 16.3 J | 10.0 - 12.0 ft-lb | Notched; 44 HRC |
Schmolz + Bickenbach Thermodur® 2343 EFS Extra Fine Structure (H-11)- Hot Work Die Steel Description: Thermodur® 2343 is a single melt Extra Fine Structure (EFS) hot work die steel and Supplied in the annealed conditionCharacteristics: Good toughness; Moderate high-temperature strength.. |
|||
Charpy Impact | 13.6 J | 10.0 ft-lb | V-Notch; Air Cooled from 941°C; 425°C Temper Temperature |
Latrobe LSS™ S7 Shock-Resisting Tool Steel (ASTM S7) TLS S7 Shock-Resisting tool steel is an air or oil hardening tool steel that is characterized by very high impact toughness. The combination of strength and high toughness makes S7 tool steel a cand.. |