Polymer Property : Charpy Impact = 9.49 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact 9.49 J
7.00 ft-lb
V-Notch
ECOMold 95 Copper Mold Material
ECOMold® copper alloys (beryllium-free) are designed specifically for plastics industry applications. ECOMold® 95 has a superior combination of thermal conductivity, hardness, and tensile strengt..
Charpy Impact 9.49 J
7.00 ft-lb
hardened at 2100°F; C-notch
Crucible Steel REX® M42 High Speed Steel, AISI M42
REX M42 is a super cobalt high speed steel which may be heat treated to HRC 68. This makes REX M42 outstanding for special purpose cutting tools, with requirements beyond the capability of general p..
Charpy Impact 9.49 J
7.00 ft-lb
As Cast
Weartech International WT-12 Cobalt Hardfacing & Wear Resistant Alloy
Applications: extrusion dies, scissor blades, saw blades, guide bars, wood cutting tools, pump sleeves, twist rolls, knivesInformation provided by Weartech International