Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact | >= 70.0 J @Temperature -50.0 °C |
>= 51.6 ft-lb @Temperature -58.0 °F |
|
Industeel URANUS® 52N+ 25 Cr Super Duplex Stainless Steel with PREN = 40 Description: URANUS® 52N+ (UR 52N+) is a super duplex stainless steel with 25% Cr and a PREN value higher than 40. The minimum guaranteed yield strength is 550 MPa which allows the designer to re.. |
|||
Charpy Impact | >= 70.0 J @Temperature -50.0 °C |
>= 51.6 ft-lb @Temperature -58.0 °F |
|
Industeel URANUS® 47N+ 25 Cr Super Duplex Stainless Steel with PREN = 40 Description: CLI - SAF 2507® is a 25.07 super duplex stainless steel with 25% Cr and a PREN value higher than 40. The minimum guaranteed yield strength is 550 MPa which allows the designer to red.. |
|||
Charpy Impact | 70.0 J @Temperature 250 °C |
51.6 ft-lb @Temperature 482 °F |
V-notch. Short transverse direction. 47 HRC |
Assab Steels DIEVAR Hot Work Steel DIEVAR is a high performance chromium-molybdenum-vanadium alloyed hot work tool steel which offers a very good resistance to heat checking, gross checking, hot wear and plastic deformation. DIEVAR i.. |
|||
Charpy Impact | 70.0 J @Temperature 250 °C |
51.6 ft-lb @Temperature 482 °F |
V-notch. Short transverse direction. 50 HRC |
Assab Steels DIEVAR Hot Work Steel DIEVAR is a high performance chromium-molybdenum-vanadium alloyed hot work tool steel which offers a very good resistance to heat checking, gross checking, hot wear and plastic deformation. DIEVAR i.. |
|||
Charpy Impact | 70.0 J | 51.6 ft-lb | Typical Toughness (long) |
Industeel SOLEIL A2 13% Cr High Strength Martensitic Stainless Steel (QT650 Heat Treatment) Description: Soleil A2 has combined Chromium (~13%) and Carbon ~0.10%) additions to provide an excellent combination of high mechanical properties and improved corrosion resistance properties. The g.. |