Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact | >= 48.8 J | >= 36.0 ft-lb | to EN 10028-7 1.4003 |
American Utility Metals Cromgard® Stainless Steel Cromgard is a low cost stainless steel, which is able to provide benefits of good weldability and formability, making it capable of fabrication by conventional techniques. It provides the benefits o.. |
|||
Charpy Impact | 48.8 J | 36.0 ft-lb | Solution treated plus 1038°C for 50 hours |
ATI Allegheny Ludlum Altemp® HX Nickel-Based superalloy Characteristics: outstanding resistance to oxidation at high temperatures, exceptional strength at elevated temperatures, good fabricability, good machinability in annealed condition, work hardening.. |