Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact | 41.0 J | 30.2 ft-lb | Austenitizing Temperature- 1190°C; Tempering Temperature- 550°C |
Crucible Steel PM M2 Tool Steel PM M2 is an improved quality tool steel compared to conventionally produced material. The powder metallurgy process results in a homogeneous microstructure exhibiting a uniform distribution of fine .. |
|||
Charpy Impact | 41.0 J @Temperature -196 °C |
30.2 ft-lb @Temperature -321 °F |
V-notch |
Carpenter Custom 450® Stainless Steel, Annealed Data provided by Carpenter Technology Corporation.Custom 450® stainless is a martensitic age-hardenable stainless steel which exhibits very good corrosion resistance (similar to that of Stainless T.. |
|||
Charpy Impact | 41.0 J | 30.2 ft-lb | |
Haynes 230® alloy plate, 8000 hours exposure at 649°C (1200°F) Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applicat.. |