Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact | 40.0 J | 29.5 ft-lb | Typical (Longitudinal) |
Industeel FORA 360 BC 360 HB Wear Resistant Steel Description: FORA 360 BC is a water quenched, abrasion resistant steel, of a hardness 360 HB. It presents at a good aptitude of implementation in particular in welding.Information provided by manufa.. |
|||
Charpy Impact | 40.0 J @Temperature 100 °C |
29.5 ft-lb @Temperature 212 °F |
|
Industeel Superplast® 350 Mold Steel SUPERPLAST® 350 offers improved machinability, improved consistency and weldability, improved thermal conductivity, with a higher hardness allowing better mechanical properties and polishability... |
|||
Charpy Impact | 40.0 J @Temperature -20.0 °C |
29.5 ft-lb @Temperature -4.00 °F |
EN 10045 |
ThyssenKrupp PAS 315 Structural Steel for Cold Forming This Material Specification applies to plates made of low carbon high strength steels with minimum yield strength values between 315 and 700 MPa1) in the thermo mechanically rolled delivery conditio.. |
|||
Charpy Impact | 40.0 J @Temperature -20.0 °C |
29.5 ft-lb @Temperature -4.00 °F |
EN 10045 |
ThyssenKrupp PAS 355 Structural Steel for Cold Forming This Material Specification applies to plates made of low carbon high strength steels with minimum yield strength values between 315 and 700 MPa1) in the thermo mechanically rolled delivery conditio.. |
|||
Charpy Impact | 40.0 J @Temperature -20.0 °C |
29.5 ft-lb @Temperature -4.00 °F |
EN 10045 |
ThyssenKrupp PAS 380 Structural Steel for Cold Forming This Material Specification applies to plates made of low carbon high strength steels with minimum yield strength values between 315 and 700 MPa1) in the thermo mechanically rolled delivery conditio.. |
|||
Charpy Impact | 40.0 J @Temperature -20.0 °C |
29.5 ft-lb @Temperature -4.00 °F |
EN 10045 |
ThyssenKrupp PAS 420 Structural Steel for Cold Forming This Material Specification applies to plates made of low carbon high strength steels with minimum yield strength values between 315 and 700 MPa1) in the thermo mechanically rolled delivery conditio.. |
|||
Charpy Impact | 40.0 J @Temperature -20.0 °C |
29.5 ft-lb @Temperature -4.00 °F |
EN 10045 |
ThyssenKrupp PAS 460 Structural Steel for Cold Forming This Material Specification applies to plates made of low carbon high strength steels with minimum yield strength values between 315 and 700 MPa1) in the thermo mechanically rolled delivery conditio.. |
|||
Charpy Impact | 40.0 J @Temperature -20.0 °C |
29.5 ft-lb @Temperature -4.00 °F |
EN 10045 |
ThyssenKrupp PAS 500 Structural Steel for Cold Forming This Material Specification applies to plates made of low carbon high strength steels with minimum yield strength values between 315 and 700 MPa1) in the thermo mechanically rolled delivery conditio.. |
|||
Charpy Impact | 40.0 J @Temperature -20.0 °C |
29.5 ft-lb @Temperature -4.00 °F |
EN 10045 |
ThyssenKrupp PAS 550 Structural Steel for Cold Forming This Material Specification applies to plates made of low carbon high strength steels with minimum yield strength values between 315 and 700 MPa1) in the thermo mechanically rolled delivery conditio.. |
|||
Charpy Impact | 40.0 J @Temperature -20.0 °C |
29.5 ft-lb @Temperature -4.00 °F |
EN 10045 |
ThyssenKrupp PAS 600 Structural Steel for Cold Forming This Material Specification applies to plates made of low carbon high strength steels with minimum yield strength values between 315 and 700 MPa1) in the thermo mechanically rolled delivery conditio.. |
|||
Charpy Impact | 40.0 J @Temperature -20.0 °C |
29.5 ft-lb @Temperature -4.00 °F |
EN 10045 |
ThyssenKrupp PAS 650 Structural Steel for Cold Forming This Material Specification applies to plates made of low carbon high strength steels with minimum yield strength values between 315 and 700 MPa1) in the thermo mechanically rolled delivery conditio.. |
|||
Charpy Impact | 40.0 J @Temperature -20.0 °C |
29.5 ft-lb @Temperature -4.00 °F |
EN 10045 |
ThyssenKrupp PAS 700 Structural Steel for Cold Forming This Material Specification applies to plates made of low carbon high strength steels with minimum yield strength values between 315 and 700 MPa1) in the thermo mechanically rolled delivery conditio.. |
|||
Charpy Impact | 40.0 J | 29.5 ft-lb | Austenitizing Temperature- 1065°C |
Crucible Steel Cru-Wear® Tool Steel CRU-WEAR is an air-hardening tool steel, heat treatable to HRC 60-65. Designed as an upgrade to D2, it offers better wear resistance, greater toughness and higher attainable hardness. Compared to th.. |