Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact | 38.0 J | 28.0 ft-lb | Hardening Temperature- 1165°C; Tempering Temperature- 565°C |
Crucible Steel CPM® Rex M4 HC(HS) Tool Steel CPM REX M4 HC(HS) is a high vanadium special purpose high speed steel exhibiting better wear resistance and toughness than M2 or M3 in cold work punches, die inserts and cutting applications involvi.. |
|||
Charpy Impact | 38.0 J | 28.0 ft-lb | V-Notch, Hardened at 1850°F for 30 min, oil quenched and tempered for 4 hrs at 500°F [9.5 mm plate, transverse] |
AK Steel 410 Cb Martensitic Stainless steel AK Steel 410 Cb is an improved version of standard Type 410. The addition of columbium offers 3 major advantages: 1) Greater ease in heat treating, 2) Higher strength and toughness, 3) Improved gra.. |
|||
Charpy Impact | 38.0 J | 28.0 ft-lb | |
Haynes 230® alloy plate, 16000 hours exposure at 649°C (1200°F) Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applicat.. |