Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact | 35.0 J @Temperature -20.0 °C |
25.8 ft-lb @Temperature -4.00 °F |
Typical |
Industeel FORA 400 400 HB Wear Resistant Steel Description: FORA 400 is a water quenched martensitic steel, with a typical hardness of 400HB (42.5 HRC), constituting a real answer to abrasive wear. Thanks to its toughness, its elevated hardness,.. |
|||
Charpy Impact | 35.0 J | 25.8 ft-lb | Guaranteed in T Direction |
Industeel VIRGO 39 16% Cr, 5% Ni, Martensitic Stainless Steel Description: Virgo 39 is a 16% Cr, 5% Ni, 1% Mo low carbon martensitic stainless steel. The grade is specially designed to combine high mechanical properties including toughness and improved corrosi.. |
|||
Charpy Impact | 35.0 J | 25.8 ft-lb | |
Haynes 242® alloy, after 8000 hours exposure at 650°C (1200°F) Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm.. |
|||
Charpy Impact | 35.0 - 55.0 J | 25.8 - 40.6 ft-lb | Notched; as built |
EOS MS1 Maraging Steel for DMLS 3D Printing EOS Maraging Steel MS1 is a steel powder which has been optimized especially for processing on EOSINT M 270 systems. This steel has very good mechanical properties, and is easily heat-treatable us.. |
|||
Charpy Impact | 35.0 J | 25.8 ft-lb | Hardening Temperature- 1065°C; Tempering Temperature- 550°C |
Crucible Steel CPM® 10V® (AISI A11) Tool Steel CPM 10V was the first in the family of high vanadium tool steels made by the Crucible Particle Metallurgy process. Crucible engineers optimized the vanadium content to provide superior wear resistan.. |
|||
Charpy Impact | 35.0 J | 25.8 ft-lb | Hardening Temperature- 1175°C; Tempering Temperature- 550°C |
Crucible Steel CPM® 9V® Tool Steel CPM 9V is made by the Crucible Particle Metallurgy process. Its composition is a modification of CPM 10V with lower carbon and vanadium to improve toughness and heat check resistance. These enhanced.. |
|||
Charpy Impact | 35.0 J | 25.8 ft-lb | Austenitizing Temperature- 1150°C; Tempering Temperature- 580°C |
Crucible Steel PM M2 Tool Steel PM M2 is an improved quality tool steel compared to conventionally produced material. The powder metallurgy process results in a homogeneous microstructure exhibiting a uniform distribution of fine .. |
|||
Charpy Impact | 35.0 J | 25.8 ft-lb | Longitudinal, (10mmx10mm) |
Bisalloy Steels BisPlate 500 Thickness 6-100 mm A through hardened, abrasion resistant steel plate, offering long life expectancy in sliding and gouging abrasion applications.Applications: Dump Truck Wear Liners, Chutes, Wear Liners, Earth Moving.. |
|||
Charpy Impact | 35.0 J | 25.8 ft-lb | |
Haynes 230® alloy, plate, 4000 hours exposure at 871°C (1600°F) Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applicat.. |