Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact | 325 J | 240 ft-lb | Typical |
Industeel CLC 17.13.3 LN Nitrogen Containing 18Cr-10Ni-2Mo Austenitic Stainless Steel Description: CLC 17-13-3LN is a nitrogen alloyed austenitic stainless steel with Mo additions. Its low carbon content avoids intergranular corrosion, even on welded pieces without an ulterior water .. |
|||
Charpy Impact | 325 J | 240 ft-lb | 10 mm sample from annealed plate |
ATI Allegheny Ludlum AL 276™ Nickel-Base Alloy, UNS N10276 AL 276 alloy is a nickel-chromium-iron-tungsten alloy which is among the most corrosion resistant of alloys currently available. The AL 276 alloy is widely used in the severest environments encount.. |
|||
Charpy Impact | 325 J | 240 ft-lb | V-notch |
Carpenter Gall-Tough® Stainless, Annealed and Cold Drawn Bar, 0% Cold Work Data provided by Carpenter Technology Corporation.Threshold Galling Stress 103 MPa (higher stress tests not performed). The avg. total volume loss on the wear test is 5 mm³ at 100 rpm.Gall-Tough®.. |