Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact | 24.0 J | 17.7 ft-lb | |
Haynes 230® alloy, plate, 1000 hours exposure at 871°C (1600°F) Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic.. |
|||
Charpy Impact | 24.0 J | 17.7 ft-lb | aged 4000 hours at 760°C (1400°F) |
Haynes HR-160® alloy, plate, aged 4000 hours at 760°C (1400°F) Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an.. |
|||
Charpy Impact | 24.0 J | 17.7 ft-lb | Austenitizing Temperature- 1010°C, air cool, Tempering Temperature- 605°C |
Crucible Steel Nu-Die® V (AISI H13) Hot Work Tool Steel Nu-Die® V (AISI H13) has been the most popular, and perhaps the most versatile hot work tool steel available for many years. It provides a good balance of toughness, heat check resistance and tempe.. |
|||
Charpy Impact | 24.0 J | 17.7 ft-lb | Austenitizing Temperature- 1010°C, air cool, Tempering Temperature- 605°C |
Crucible Steel Nu-Die® XL (Premium Quality AISI H13) Tool Steel Nu-Die XL (AISI H13) is a premium version of H13 tool steel manufactured, tested and certified to meet stringent die casting industry specifications issued by NADCA, Chrysler and others. It offers b.. |
|||
Charpy Impact | 24.0 J | 17.7 ft-lb | |
Haynes 230® alloy, plate, 1000 hours exposure at 760°C (1400°F) Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applicat.. |
|||
Charpy Impact | 24.0 J | 17.7 ft-lb | |
Latrobe Staminal™ Shock Resisting Die Steel Staminal is an air or oil hardening die steel containing a large percentage of nickel combined with a proper balance of other alloying elements for deep hardening and extreme toughness. For tools, .. |