Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact | >= 150 J | >= 111 ft-lb | |
Industeel CLC 18.10 Nb Niobium Stabilized 18Cr-10Ni Austenitic Stainless Steel CLC 18-10Nb is a 18Cr-10Ni austenitic stainless steel stabilized with specific Nb addition. This kind of steel is one of the basic grades of the stainless steels range. Niobium bearing and its low c.. |
|||
Charpy Impact | >= 150 J | >= 111 ft-lb | |
Industeel CLC 18.10Ti Titanium-Stabilized 18Cr-10Ni Austenitic Stainless Steel CLC 18-10Ti is a 18Cr-9Ni austenitic stainless steel stabilized with some Titanium additions. This is a basic grades in the stainless steel range. Titanium bearing (carbide forming element) avoids i.. |
|||
Charpy Impact | 150 J | 111 ft-lb | Typical |
Industeel URANUS® 35N 23.04 Duplex Stainless Steel with PREN = 24 Description: URANUS® 35N (UR 35N) is a 23% Cr, 4% Nickel, Mo free duplex stainless steel (23.04). The alloy UR 35N has similar corrosion resistance properties similar to 316L. Furthermore, its me.. |
|||
Charpy Impact | 150 J | 111 ft-lb | |
ATI Allegheny Ludlum Stainless Steel Type 301, 3/4 Hard (UNS S30100) Allegheny Ludlum Type 301 is a high strength grade of steel available in six conditions or tempers, its resistance to atmosphere corrosion and its bright, attractive surface make it an excellent cho.. |
|||
Charpy Impact | 150 J @Temperature -73.0 °C |
111 ft-lb @Temperature -99.4 °F |
|
ATI Allegheny Ludlum Stainless Steel Type 301, 3/4 Hard (UNS S30100) Allegheny Ludlum Type 301 is a high strength grade of steel available in six conditions or tempers, its resistance to atmosphere corrosion and its bright, attractive surface make it an excellent cho.. |
|||
Charpy Impact | 150 J @Temperature 196 °C |
111 ft-lb @Temperature 385 °F |
|
ATI Allegheny Ludlum Stainless Steel Type 301, 3/4 Hard (UNS S30100) Allegheny Ludlum Type 301 is a high strength grade of steel available in six conditions or tempers, its resistance to atmosphere corrosion and its bright, attractive surface make it an excellent cho.. |
|||
Charpy Impact | 150 J | 111 ft-lb | Typical |
ATI Allegheny Ludlum AL 601™ Nickel-Base Alloy, Annealed at 982°C (1800°F), UNS N06601 Allegheny Ludlum's AL 601 alloy is an austenitic nickel-chromium-iron alloy designed for both heat and corrosion resistance. As compared to AL 600 alloy, the AL 601 alloy has, in addition to increa.. |
|||
Charpy Impact | 150 J | 111 ft-lb | |
ATI Allegheny Ludlum Stainless Steel Type 301, 1/2 Hard (UNS S30100) Allegheny Ludlum Type 301 is a high strength grade of steel available in six conditions or tempers, its resistance to atmosphere corrosion and its bright, attractive surface make it an excellent cho.. |
|||
Charpy Impact | 150 J @Temperature -73.0 °C |
111 ft-lb @Temperature -99.4 °F |
|
ATI Allegheny Ludlum Stainless Steel Type 301, 1/2 Hard (UNS S30100) Allegheny Ludlum Type 301 is a high strength grade of steel available in six conditions or tempers, its resistance to atmosphere corrosion and its bright, attractive surface make it an excellent cho.. |
|||
Charpy Impact | 150 J @Temperature 196 °C |
111 ft-lb @Temperature 385 °F |
|
ATI Allegheny Ludlum Stainless Steel Type 301, 1/2 Hard (UNS S30100) Allegheny Ludlum Type 301 is a high strength grade of steel available in six conditions or tempers, its resistance to atmosphere corrosion and its bright, attractive surface make it an excellent cho.. |
|||
Charpy Impact | 150 J | 111 ft-lb | |
ATI Allegheny Ludlum Stainless Steel Type 301, 1/4 Hard (UNS S30100) Allegheny Ludlum Type 301 is a high strength grade of steel available in six conditions or tempers, its resistance to atmosphere corrosion and its bright, attractive surface make it an excellent cho.. |
|||
Charpy Impact | 150 J @Temperature -73.0 °C |
111 ft-lb @Temperature -99.4 °F |
|
ATI Allegheny Ludlum Stainless Steel Type 301, 1/4 Hard (UNS S30100) Allegheny Ludlum Type 301 is a high strength grade of steel available in six conditions or tempers, its resistance to atmosphere corrosion and its bright, attractive surface make it an excellent cho.. |
|||
Charpy Impact | 150 J @Temperature 196 °C |
111 ft-lb @Temperature 385 °F |
|
ATI Allegheny Ludlum Stainless Steel Type 301, 1/4 Hard (UNS S30100) Allegheny Ludlum Type 301 is a high strength grade of steel available in six conditions or tempers, its resistance to atmosphere corrosion and its bright, attractive surface make it an excellent cho.. |
|||
Charpy Impact | 150 J | 111 ft-lb | |
ATI Allegheny Ludlum Stainless Steel Type 301, annealed (UNS S30100) Allegheny Ludlum Type 301 is a high strength grade of steel available in six conditions or tempers, its resistance to atmosphere corrosion and its bright, attractive surface make it an excellent cho.. |
|||
Charpy Impact | 150 J @Temperature -73.0 °C |
111 ft-lb @Temperature -99.4 °F |
|
ATI Allegheny Ludlum Stainless Steel Type 301, annealed (UNS S30100) Allegheny Ludlum Type 301 is a high strength grade of steel available in six conditions or tempers, its resistance to atmosphere corrosion and its bright, attractive surface make it an excellent cho.. |
|||
Charpy Impact | 150 J @Temperature 196 °C |
111 ft-lb @Temperature 385 °F |
|
ATI Allegheny Ludlum Stainless Steel Type 301, annealed (UNS S30100) Allegheny Ludlum Type 301 is a high strength grade of steel available in six conditions or tempers, its resistance to atmosphere corrosion and its bright, attractive surface make it an excellent cho.. |
|||
Charpy Impact | 150 J | 111 ft-lb | |
ATI Allegheny Ludlum Stainless Steel Type 301, Full Hard (UNS S30100) Allegheny Ludlum Type 301 is a high strength grade of steel available in six conditions or tempers, its resistance to atmosphere corrosion and its bright, attractive surface make it an excellent cho.. |
|||
Charpy Impact | 150 J @Temperature -73.0 °C |
111 ft-lb @Temperature -99.4 °F |
|
ATI Allegheny Ludlum Stainless Steel Type 301, Full Hard (UNS S30100) Allegheny Ludlum Type 301 is a high strength grade of steel available in six conditions or tempers, its resistance to atmosphere corrosion and its bright, attractive surface make it an excellent cho.. |
|||
Charpy Impact | 150 J @Temperature 196 °C |
111 ft-lb @Temperature 385 °F |
|
ATI Allegheny Ludlum Stainless Steel Type 301, Full Hard (UNS S30100) Allegheny Ludlum Type 301 is a high strength grade of steel available in six conditions or tempers, its resistance to atmosphere corrosion and its bright, attractive surface make it an excellent cho.. |
|||
Charpy Impact | 150 J | 111 ft-lb | Typical |
Industeel URANUS® 45N 22Cr 3Mo Duplex Stainless Steel with PREN = 33 or 34 Description: URANUS® 45N (UR 45N) is a nitrogen alloyed (= 0.15%) austenitic-ferritic stainless steel (22.05 type) with improved structure stability and high general, localized and stress corrosion.. |