Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact | 105 J @Temperature 400 °C |
77.4 ft-lb @Temperature 752 °F |
V-notch. Short transverse direction. 45 HRC |
Assab Steels DIEVAR Hot Work Steel DIEVAR is a high performance chromium-molybdenum-vanadium alloyed hot work tool steel which offers a very good resistance to heat checking, gross checking, hot wear and plastic deformation. DIEVAR i.. |