Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Fatigue Strength | 270 MPa @# of Cycles 9.00e+6 |
39200 psi @# of Cycles 9.00e+6 |
R=-1; Kt=1; 50 Hz |
CRP Technology 8601 Aerospace Grade Power Metallurgy Aluminum Alloy For Motorsport and Aerospace marketplaces: manufactured by a special powder metallurgy process using a high-energy mixing process which ensures excellent mechanical properties.Super Aluminium materi.. |
|||
Fatigue Strength | <= 270 MPa @# of Cycles 1.00e+6 |
<= 39200 psi @# of Cycles 1.00e+6 |
|
ArcelorMittal 05 High formability steel for drawing, Cold rolled Available in the following: uncoated (DC05) and electroglavanized (DC05+ZE) Description: This range of non-alloyed mild steels is designed for deep and extra deep drawing applications. These product.. |