Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Fatigue Strength | 117 MPa @# of Cycles 1.00e+7 , Temperature 593 °C |
17000 psi @# of Cycles 1.00e+7 , Temperature 1100 °F |
|
AK Steel 409 Ferritic Stainless steel AK Steel 409 Stainless Steels are especially useful for applications where oxidation or corrosion protection beyond the capacity of carbon steel and some coated steels is needed. Current applicatio.. |