Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Fatigue Strength | 450 MPa @# of Cycles 1.00e+7 |
65300 psi @# of Cycles 1.00e+7 |
Rod, rotating bend (UTS = 791 Mpa) |
TIMET TIMETAL® 230 Titanium Alloy (Ti-2.5Cu); STA Cold Formable Medium-Strength AlloyFeatures: This binary, age hardening alloy combines the easy formability and weldability of commercially pure titanium with improved mechanical properties, particu.. |
|||
Fatigue Strength | <= 450 MPa @# of Cycles 2.00e+6 |
<= 65300 psi @# of Cycles 2.00e+6 |
|
ArcelorMittal FB 560 Hot rolled ferrite-bainite steel Available in the following: Extragal® (HDT560F+Z)Description: This range of hot-rolled high strength steels has been developed to meet weight reduction requirements. It comprises four strength leve.. |
|||
Fatigue Strength | <= 450 MPa @# of Cycles 1.00e+7 |
<= 65300 psi @# of Cycles 1.00e+7 |
|
ArcelorMittal FB 560 Hot rolled ferrite-bainite steel Available in the following: Extragal® (HDT560F+Z)Description: This range of hot-rolled high strength steels has been developed to meet weight reduction requirements. It comprises four strength leve.. |