Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Fatigue Strength | 40.0 MPa @# of Cycles 100000 |
5800 psi @# of Cycles 100000 |
|
BASF Ultrason S 3010 PSU Ultrason S 3010 is an unreinforced, higher viscosity injection molding and extrusion PSU grade, tougher and with improved chemical resistance. It conforms to FDA requirements of 21 CFR 177.1655. |