Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Fatigue Strength | 330 MPa @# of Cycles 200000 |
47900 psi @# of Cycles 200000 |
R=-1; Kt=1; 50 Hz |
CRP Technology 8601 Aerospace Grade Power Metallurgy Aluminum Alloy For Motorsport and Aerospace marketplaces: manufactured by a special powder metallurgy process using a high-energy mixing process which ensures excellent mechanical properties.Super Aluminium materi.. |