Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Fatigue Strength | 296 MPa @# of Cycles 1.00e+6 |
43000 psi @# of Cycles 1.00e+6 |
|
American Utility Metals Cromgard® Stainless Steel Cromgard is a low cost stainless steel, which is able to provide benefits of good weldability and formability, making it capable of fabrication by conventional techniques. It provides the benefits o.. |
|||
Fatigue Strength | 296 MPa @# of Cycles 4.00e+6 |
43000 psi @# of Cycles 4.00e+6 |
|
American Utility Metals Cromgard® Stainless Steel Cromgard is a low cost stainless steel, which is able to provide benefits of good weldability and formability, making it capable of fabrication by conventional techniques. It provides the benefits o.. |
|||
Fatigue Strength | 296 MPa @# of Cycles 1.00e+7 , Temperature 454 °C |
42900 psi @# of Cycles 1.00e+7 , Temperature 849 °F |
|
AK Steel 410 Martensitic Stainless steel AK Steel 410 provides good corrosion resistance plus high strength and hardness. It is magnetic in both annealed and hardened conditions. A wide range of properties can be developed with different.. |