Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Fatigue Strength | 1200 MPa @# of Cycles 20000 |
174000 psi @# of Cycles 20000 |
|
International Mold Steel Daido DRM2 Matrix High-Speed Steel This matrix type high speed tool steel is available for warm and cold forging tools where critical performance is required. DRM2 prolongs service life due to its higher hardness and toughness than t.. |