Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 6.60 - 520 GPa | 957 - 75400 ksi | Average value: 105 GPa Grade Count:59 |
Overview of materials for Epoxy/Carbon Fiber Composite This property data is a summary of similar materials in the MatWeb database for the category "Epoxy/Carbon Fiber Composite". Each property range of values reported is minimum and maximum values of a.. |