Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 1.38 - 46.0 GPa | 200 - 6670 ksi | Average value: 19.2 GPa Grade Count:16 |
Overview of materials for Epoxy Molding Compound This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Molding Compound". Each property range of values reported is minimum and maximum values of appropr.. |